gptkbp:instanceOf
|
aluminum alloy
|
gptkbp:alsoKnownAs
|
gptkb:Inconel_600
gptkb:Alloy_600
|
gptkbp:application
|
aerospace
food processing
nuclear reactors
chemical processing
heat treating equipment
|
gptkbp:chromiumContent
|
14-17%
|
gptkbp:component
|
iron
nickel
chromium
|
gptkbp:corrosionResistance
|
high
|
gptkbp:countryOfOrigin
|
gptkb:United_States
|
gptkbp:creepResistance
|
good
|
gptkbp:density
|
8.47 g/cm³
|
gptkbp:elongation
|
30% minimum
|
gptkbp:formability
|
good
|
https://www.w3.org/2000/01/rdf-schema#label
|
UNS N06600
|
gptkbp:ironContent
|
6-10%
|
gptkbp:magnetType
|
non-magnetic
|
gptkbp:mainVendors
|
gptkb:Special_Metals_Corporation
|
gptkbp:meltingPoint
|
1354°C
|
gptkbp:nickelContent
|
72% minimum
|
gptkbp:oxidationResistance
|
high
|
gptkbp:resistantTo
|
organic acids
alkalis
chloride-ion stress corrosion cracking
oxidizing conditions
reducing conditions
|
gptkbp:standardizedBy
|
gptkb:ASTM_B163
gptkb:ASTM_B166
gptkb:ASTM_B167
gptkb:ASTM_B168
ASTM B751
ASTM B775
ASTM B829
|
gptkbp:stressCorrosionCrackingResistance
|
good
|
gptkbp:tensileStrength
|
550 MPa minimum
|
gptkbp:trademarkOf
|
gptkb:Inconel
|
gptkbp:UNNumber
|
N06600
|
gptkbp:usedFor
|
nuclear reactor components
chemical plant equipment
furnace components
steam generator tubing
thermocouple sheaths
|
gptkbp:weldability
|
good
|
gptkbp:yield
|
205 MPa minimum
|
gptkbp:bfsParent
|
gptkb:Inconel_600
gptkb:ASTM_B163
|
gptkbp:bfsLayer
|
7
|