Statements (32)
Predicate | Object |
---|---|
gptkbp:instanceOf |
gptkb:steel
high-yield steel |
gptkbp:composedOf |
carbon
iron nickel manganese silicon molybdenum chromium |
gptkbp:corrosionResistance |
moderate
|
gptkbp:density |
7.85 g/cm³
|
gptkbp:developedBy |
gptkb:United_States_Navy
|
gptkbp:heatTreatment |
quenched and tempered
|
https://www.w3.org/2000/01/rdf-schema#label |
HY-80 steel
|
gptkbp:meltingPoint |
1425–1510 °C
|
gptkbp:notableFor |
toughness
high strength weldability |
gptkbp:standardizedBy |
gptkb:ASTM_A372
gptkb:MIL-S-16216 |
gptkbp:tensileStrength |
100,000–120,000 psi
|
gptkbp:usedBy |
gptkb:Royal_Navy
gptkb:United_States_Navy other navies |
gptkbp:usedIn |
naval vessels
pressure vessels offshore structures submarine hulls |
gptkbp:weldability |
good
|
gptkbp:yield |
80,000 psi
|
gptkbp:bfsParent |
gptkb:marine
|
gptkbp:bfsLayer |
4
|